Advanced Modeling Methods for Pitting Corrosion in Metals
185,70 €
Taylor & Francis Ltd
Sivumäärä: 304 sivua
Asu: Kovakantinen kirja
Julkaisuvuosi: 2026, 30.03.2026 (lisätietoa)
Kieli: Englanti
Pitting corrosion poses a significant threat to infrastructure in engineering and there is a lack of comprehensive modeling methodologies to assess the effectiveness of corrosion mitigation strategies specifically designed for various structural systems. This book addresses the need for comprehensive, advanced models that integrate the various stages and factors involved in the process. It covers corrosion fatigue mechanisms and the influence of stress and temperature, and ways to mitigate corrosion induced damage in structural components.



Discusses exclusive material on modeling of the pitting corrosion process
Provides a brief outline of experimental techniques for pitting corrosion
Advanced numerical modeling techniques are explained with a number of examples
Presents data on modular form for easy understanding of the modeling techniques
Includes equations/flow charts to generate the numerical codes

This book is a reference for scholars, educators, and practitioners interested in exploring the potential of CPS for inclusive rural development.

LISÄÄ OSTOSKORIIN
Tuotetta lisätty
ostoskoriin kpl
Siirry koriin
Tilaustuote

Tilaustuote

Tämän tuotteen tilaamme kustantajalta tai tukkurilta varastoomme. Saatavuusarvio on tuotekohtainen. Lähetämme toimitusvahvistuksen heti, kun tuote on toimitettu varastoltamme rahdinkuljettajalle.

Arvioimme, että tuote lähetetään meiltä noin 1-3 viikossa.
Myymäläsaatavuus
Helsinki
Tapiola
Turku
Tampere
Advanced Modeling Methods for Pitting Corrosion in MetalsSuurenna kuva
Näytä kaikki tuotetiedot
ISBN:
9781041068310
Kansikuva tuotteelle